Standardization field | Metallic materials |
Technical committee | BAS/TC 4- Steel, steel products, non-ferrous metals and alloys |
Term (EN) | stress relief tempering |
Definition (EN) | TEMPERING carried out at a temperature generally below 200 oC on totally or partially martensitic structures in order to reduce the intrinsic stresses by the onset of carbide precipitation without too much reduction in the hardness.
|
Term (FR) | |
Definition (FR) | |
Term (DE) | |
Definition (DE) | |
Term (BS) | protunaponsko popuštanje |
Definition (BS) | POPUŠTANJE koje se vrši na temperaturi općenito ispod 200 oC na potpunu ili djelimičnu martenzitnu strukturu u cilju smanjenja unutarnjih naprezanja putem početka precipitacije karbida bez prevelikog smanjenja tvrdoće.
|
Term (HR) | |
Definition (HR) | |
Term (SR) | |
Definition (SR) | |
Date | 2016-04-04 |
Standards | BAS EN 10052:2005 |
---|