prBAS EN 13036-8:2026
Road and airfield surface characteristics - Test methods - Part 8: Determination of transverse unevenness and crossfall indices
Opće informacije
Status:Projekt
Broj stranica:40
Metoda usvajanja:Proglašavanje
Jezik:engleski
Izdanje:2.
Nadnevak realizacije:07.11.2025
Predviđeni nadnevak naredne faze:27.11.2025
Tehnički komitet:BAS/TC 22, Cestogradnja
ICS:
93.080.10, Tehnika gradnje cesta
93.120, Gradnja aerodroma
93.120, Gradnja aerodroma
Apstrakt
This document specifies the mathematical processing of digitized transverse profile measurements to produce indices in the transverse direction for unevenness, other defects and crossfall. The document describes the calculation methods of the indices, such as irregularities, (1) rut depth, (2) ridge height, (3) water depth and area, (4) crossfall, and how to evaluate and report the indices. It also describes possibilities to do further analysis to examine defects and problems on the road that can be seen in the transverse profile. The latter is described in Annex E.
Životni ciklus
...
Izvorni dokument i stepen usklađenosti
EN 13036-8:2025, identičan
Veza sa BAS standardima
Radni materijal
Samo članovi tehničkog komiteta imaju pristup radnom materijalu. Ukoliko ste član, molimo prijavite se sa vašim nalogom i dobićete pristup dokumentima. Пријавите се